High strength casting material is made of high quality bauxite aggregate, powder and additive and binder in a reasonable distribution which is mixed with. Each bag of 40kg, the mixture and binder (1 bags) two parts. To tell you the scene of simple technology.
1. The castable materials with forced mixer mixing.
2. The proportion of castable:
The mixture ratio of water binder: amount of 95:5: 8%-10.5%.
Note: the amount of water can be reasonably adjusted according to the seasons, temperature and actual operation situation.
3. Mixed castable:
The mix material and binder quantitative (a pouch in each bag) poured into the mixer dry mixing minutes, then adding quantitative clean tap water wet mix two to three minutes, moderate humidity can be expected.